Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Victrex PEEK - PEEK - Victrex plc

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Victrex PEEK" in Material Data Center leads to the following information:

Tradename: Victrex PEEK
Family: PEEK
Producer: Victrex plc
43 hits in the material database
22 hits in the literature database
22 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Application
VICTREX® PEEK Hub caps, Boeing 777
VICTREX® PEEK USB stick
VICTREX® PEEK Clamps
VICTREX® PEEK Hub cap, landing gear of the Boeing 747-8
VICTREX® PEEK Valve clip, RSD hydraulic coupling
VICTREX® PEEK Robot speed reducers
VICTREX® PEEK Bite-stick
VICTREX® PEEK Metapot sensor
VICTREX® PEEK Filling valves, beverage bottling machine
VICTREX® PEEK Bearing cage
VICTREX® PEEK Electronic coupling, plasma TV
VICTREX® PEEK X-ray tablet clamps
VICTREX® PEEK Electrical connectors
VICTREX® PEEK Insulation for power connector
VICTREX® PEEK 450GL30 Valve plate, reciprocating compressor
VICTREX® PEEK Fuel housing for the aircraft industry
VICTREX® PEEK-ESD™ Aerospace brackets
VICTREX® PEEK 90HMF40 Fitting in the aircraft door of the Airbus A350-900
VICTREX® PEEK Subsea intervention line
VICTREX® PEEK Inner water tank, mobile drink dispenser
VICTREX® PEEK HPHT Electrical Connector
VICTREX® PEEK 90HMF40 Drive-Shaft system

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.